Gelling of chips during vertical surface diamond grinding of BK7 glass
n this work diamond pins of diameter 5 mm were used to produce plano surfaces on glass by vertical surface grinding on a 3-axis CNC machining centre. Chip clearance appeared to be difficult and led to the formation of stalling and zero velocity tracks, which continued to persist even after polishing...