Phase formation during reduction of iron sand with soda ash flux addition
Iron sand deposit in Indonesia generally consisted of titanomagnetite with ilmenite lamelaa occurred in magnetite particle structure, therefore direct physical separation through magnetic method at particle size of 400 mesh only capable increasing total iron content up to 60%. In order to increas...