Cold formed steel and buckling criteria of cold formed steel purlins / Fadhluhartini Muftah and Mohd Syahrul Hisyam Mohd Sani
Cold formed steel member made up at room temperatures which cause the material may become harder and stronger. Generally there are two method of producing cold formed steel either by press breaking or cold forming depending on type and capacity of section required. Cold formed steel can be use...
Saved in:
| Main Authors: | , |
|---|---|
| Format: | Conference or Workshop Item |
| Language: | English |
| Published: |
2009
|
| Subjects: | |
| Online Access: | http://ir.uitm.edu.my/11017/ http://ir.uitm.edu.my/11017/1/PRO_FADHLUHARTINI%20MUFTAH%20C%2009.pdf |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
| Summary: | Cold formed steel member made up at room temperatures which cause the material
may become harder and stronger. Generally there are two method of producing cold
formed steel either by press breaking or cold forming depending on type and capacity
of section required. Cold formed steel can be used either in general application or
building application due to several advantages such as high strength, lightweight and
cost-effective way of covering a wide variety of building structures. |
|---|