Relationships between compressive strength of cement-slag mortars under air and water curing regimes
In this investigation 12 mortar mixes including three groups were prepared using binder contents 380 and 500 kg/m 3. All the specimens were cured after casting and demoulding in curing regimes, i.e. at room temperature (ac) and in water (wc). The highest strength was obtained for cement-slag mortars...
Saved in:
因特网
http://www.scopus.com/inward/record.url?eid=2-s2.0-84856044706&partnerID=40&md5=845dbbdb848446d702f16049c519865a www.sciencedirect.com/science/article/pii/S0950061811007355 http://ac.els-cdn.com/S0950061811007355/1-s2.0-S0950061811007355-main.pdf?tid=2602http://www.scopus.com/inward/record.url?eid=2-s2.0-84856044706&partnerID=40&md5=845dbbdb848446d702f16049c519865a www.sciencedirect.com/science/article/pii/S0950061811007355 http://ac.els-cdn.com/S0950061811007355/1-s2.0-S0950061811007355-main.pdf?tid=2602